Defects can be grouped under three main
classifications
Planar Defects: linear from at least one dimension
  • Cracks.
  • Lack of fusion.
  • Linear Volumetric Defects: Linear in length with volume.
  • Slag lines.
  • lack of fusion with associated slag.
  • Piping.
  • Non-planar defects: rounded indications without significat length.
  • Slag inclusions.
  • Gas pores/blow holes.
  • Other matallic and non-matallic inclusions.
http://adf.ly/iv0NR





Setelah download rubah  : *. pdf  > *.zip

.

7 komentar :

could you please confirm how this file is downloaded becouse the down load title is not efficiently active

Download it first then *. Pdf converted into *. Rar

i downloaded the file below the video as pdf format and it does not work like the video.......what can i do please .

dear admin,

the link has broken please shared updated, it will help for my exam :)

Posting Komentar

Related Posts Plugin for WordPress, Blogger...

Tags

Translate

Ipaluni Atevet Bulldozer Headline Animator

Jam

Total Tayangan Halaman

Sitemap

Blog Archive

Blog Archive